On Uncertainty of Elastic Modulus Measurements via Nanoindentation Mechanical Testing and Conventional Triaxial Testing
Published in Journal of Rock Mechanics and Geotechnical Engineering, 2025
Recommended citation: Wu, Z., Edelman, E., Ritterbush, K., McPherson, B. (2025). "On Uncertainty of Elastic Modulus Measurements via Nanoindentation Mechanical Testing and Conventional Triaxial Testing." Journal of Rock Mechanics and Geotechnical Engineering.